Walk into a lumberyard and ask for hardwood, and you will hear terms like “FAS,” “Select,” and “No. 1 Common.” Ask for pine, and suddenly it is “Select,” “Premium,” or “Stud Grade.” Same words, different meanings. It is genuinely confusing, and it costs beginners money when they buy the wrong grade for the job.
Both systems come down to the same question asked from different angles: how much clear, usable wood is in the board, or how strong it is. Sort out which system you are looking at and what each grade actually buys you, and you stop overpaying for premium boards when a common grade would do, while still knowing the times the upgrade is worth it.
Two Different Grading Systems
The lumber industry uses completely separate grading standards for hardwoods and softwoods. That is not arbitrary; it reflects how the two are used and sold.
Hardwoods like oak, maple, cherry, and walnut are graded by the National Hardwood Lumber Association. The grades measure how much clear, defect-free wood you can cut from each board, and hardwood is typically sold rough, in random widths and lengths, so you are buying raw material and milling it yourself. Softwoods like pine, fir, cedar, and spruce are graded by regional associations under standards from the American Lumber Standard Committee, focused on structural strength and appearance, and are usually sold already surfaced on four sides in standard dimensions.
The practical upshot is that “Select” hardwood and “Select” softwood are entirely different products with different characteristics and pricing. Knowing which system applies to the board in your hands is what prevents an expensive mistake at the yard.
Hardwood Grades (FAS, Select, Common)
Hardwood grades measure one thing: what percentage of the board can be cut into clear sections, called cuttings, of certain minimum sizes. Higher grades mean more clear wood per board and in larger pieces, not necessarily better or stronger wood. A knotty Common board can be every bit as sound as an FAS one; it just yields less clear material in smaller chunks.
FAS (Firsts and Seconds)
This is the top hardwood grade. FAS boards must yield at least 83.3% clear wood in pieces no smaller than 4 inches wide by 5 feet long, or 3 inches by 7 feet. In practice they are nearly clear on both faces, with only small tight knots if any, consistent color, and fairly straight grain, usually 6 inches wide or wider and 8 to 12 feet long.
Buy FAS when you need long, wide, clear sections with no character marks allowed: tabletops, wide panels, prominent visible surfaces, and book-matched boards where the figure has to run uninterrupted. Expect to pay 40 to 80% more than No. 1 Common in the same species.
Select
Select grade is identical to FAS on one face and allows more defects on the back. You get the same clear yield, but only from the good side, while the reverse face may carry knots or color variation. That makes it the smart buy for cabinet doors, drawer fronts, and any part where only one side shows, and for painted work where the hidden face does not matter. It usually runs 10 to 20% under FAS, still above No. 1 Common.
No. 1 Common
No. 1 Common requires only 66.7% clear yield in smaller pieces, at least 4 inches by 2 feet or 3 inches by 3 feet. You get shorter clear sections and more boards with character: sound tight knots, sapwood-to-heartwood color variation, narrower average widths around 4 to 6 inches, and more waste as you cut around the flaws. For smaller projects, parts that get cut into short lengths like spindles, drawer sides, and face frames, or work where you actually want character marks, it is the value grade, often 40 to 60% cheaper than FAS. Careful layout when buying rough lumber is what lets you work around defects and capture that saving.
No. 2 Common and Below
No. 2 Common (50% clear yield) and No. 3 Common (33.3%) see limited use in fine woodworking. They work for painted projects, rustic furniture, or when you are deliberately after heavily figured or distressed material, but the waste factor is high enough that you might use less than half of what you buy.
| Hardwood grade | Minimum clear yield | Best for |
|---|---|---|
| FAS | 83.3% | tabletops, wide clear panels |
| Select | 83.3% (one face) | show-face parts, doors |
| No. 1 Common | 66.7% | value pick, small parts |
| No. 2 Common | 50% | painted, rustic |
| No. 3 Common | 33.3% | limited use, high waste |
๐ณ Quality Hardwood Lumber
Online hardwood retailers often carry better grades and a wider selection than a local yard, with shipping that can beat the drive to a specialty mill. Knowing the grade you actually need keeps you from overpaying for FAS when Common would do.
Shop Hardwood LumberSoftwood Grades (Select, Common, Construction)
Softwood grading splits into two families: appearance grades for visible work like trim and furniture, and structural grades for framing. The standards come from several regional associations but line up closely.
Appearance Grades
C Select and D Select are the top appearance grades. C Select allows only tiny, tight pin knots; D Select allows slightly larger ones but still very few. Both suit clear finishes where you want minimal character, and both are expensive and often special-order. Big-box stores also sell hand-picked boards under marketing names like Premium and Supreme, which approximate Select grade at two to three times the price of standard construction lumber. The workhorse appearance grade at retail is No. 2 and Better, which allows sound knots up to roughly 1.5 inches and minor defects; it is well suited to painted work or a rustic look and costs far less than the Select grades.
Structural Grades
Select Structural is the strongest structural grade for dimension lumber, with dense tight grain and high strength ratings, used for headers, beams, and critical loads, and rarely needed for basic framing. No. 1 and No. 2 are the standard framing grades: No. 1 has tighter knot limits, but No. 2 meets code for most residential framing and is what contractors use for walls, floors, and roofs, graded for strength rather than looks. Stud Grade is graded specifically for vertical wall studs, straighter than standard No. 2 but allowing larger knots since a stud carries load vertically, and it is the default for framing walls. Below those sit Utility and Economy, high in knots and defects and suitable only for non-critical bracing or temporary work.
For painted pine furniture, this is where the money hides: No. 2 grade costs a fraction of Premium and, once it is primed and painted, looks identical. Fill any knots before painting and nobody will ever know the difference.
What Actually Determines Grade
Knowing what graders look at helps you evaluate lumber yourself and spot boards that punch above their grade.
Knots are the primary factor. Size, type, and location all matter: sound tight knots beat loose knots or knot holes, edge knots count for less than face knots, and a pin knot under a quarter inch barely registers while a 2-inch knot drops a board hard.
Grain patterns cut in a surprising direction. In hardwoods, figure like curl and quilt can lower the grade even though woodworkers prize it, because the figure disrupts clear cuttings; highly figured wood often grades as Common. In softwoods, grain slope and ring density drive the structural grades more than looks.
Color variation reduces hardwood grades. A board that is half cream sapwood and half brown heartwood grades below a uniform one, even though many builders prefer the contrast, and mineral streaks downgrade boards despite often being wanted for character.
Defects and warp round it out. Splits, checks, wane (a bark edge or missing corner), and pitch pockets all cut the grade, some disqualifying a board outright and others just limiting clear yield. Warp counts for less than you would expect, since twist, bow, cup, and crook are often milled out, though severe warp that cannot be corrected without heavy waste will downgrade lumber.
Matching Grade to Your Project
Buying the right grade for the specific job saves money without hurting the result. Match the grade to what the part has to do.
The small-parts line is the one that saves the most. When every piece is short, a wandering defect is easy to cut around, so No. 1 Common hardwood or No. 2 softwood can drop the material cost 40 to 50% with no visible difference in the finished part. The grade only has to be as good as the largest clear piece you need from it.
Cost vs. Value
Seeing the real price gaps between grades is what makes the smart-buying decisions obvious. The numbers below are illustrative and vary by region, species, and season, but the spread between grades holds fairly steady. Here is a representative set for 4/4 (one-inch) red oak.
| Grade (red oak, 4/4) | Example price / board foot | 30 bf project |
|---|---|---|
| FAS | $8.50 | $255 |
| Select | $7.00 | $210 |
| No. 1 Common | $5.00 | $150 |
| No. 2 Common | $3.50 | $105 |
If a project has parts that truly need FAS, like a tabletop, and parts where No. 1 Common works, like the base and legs, buying 20 board feet of No. 1 Common at $5.00 and 10 board feet of FAS at $8.50 comes to $185, about $70 less than buying all FAS. Splitting the buy by where the wood shows is the single easiest way to cut a lumber bill.
The catch is the waste factor: lower grades force more cutting around defects, and if you throw away 40% of a cheap board, the saving evaporates. So figure on usable yield, not sticker price. For 20 usable board feet of oak drawer parts, all under 18 inches, the FAS route is about 22 board feet at $8.50, roughly $187 with little waste, while No. 1 Common is about 28 board feet at $5.00, roughly $140 even after cutting around a quarter of it as waste. The Common route still wins here, by around $47, because the price gap is wide and the parts are short. Running the numbers through a board-foot estimate before you buy is what turns this from a guess into a decision.
๐ Lumber Measuring Essentials
Accurate board-foot math keeps you from overbuying, and a moisture meter tells you whether that bargain-grade stack is dry enough to use. Both pay for themselves quickly against the cost of wasted lumber.
Shop Lumber Rules Shop Moisture MetersShopping Smart at the Yard
Knowing the grades is only half of it. Lumber gets graded in bulk, often quickly, so a board that technically meets FAS can end up in the Select pile, and you will find exceptional No. 1 Common boards that nearly qualify as Select. Inspect every board and pick the best examples within the grade you are paying for.
When you sort, evaluate both faces, since a defect on the back may not matter for your part. Favor grain orientation that will stay put, with quartersawn the steadiest. Sight down the length for warp, remembering that minor bow is fixable but twist usually is not. Check the end grain for checks or splits running into the board. And choose boards a little longer and wider than you need, so you have room to trim defects away.
It also pays to talk to the dealer. Good lumberyards let you sort through stock and will work on price for larger orders, and explaining your project sometimes gets you steered to a lower grade that works fine, which moves their inventory and saves you money. Ask about shop grade or shorts, too; they are often heavily discounted and perfect for small parts.
Making Grade Work for You
Grades exist to standardize pricing and expectations, not to rank quality in any absolute way. A No. 1 Common board can be perfect for a job where FAS would be wasted money. Start from the project: figure out which parts truly need clear, defect-free wood and which can carry character or get painted, then buy the lowest grade that satisfies each. That habit saves money on every build and teaches you to work with wood as it actually comes, rather than paying for perfection you will cut off as offcuts anyway.
๐ซ Free Woodworking Plans for Beginners
Download step-by-step plans for beginner-friendly builds, including our popular Transformer Bench that converts from a picnic table into a bench and back again.
Download Free Plans โRead Next
Frequently Asked Questions
Does a higher grade mean stronger or better wood?
For hardwood, no. The grade measures how much clear, defect-free wood a board yields and in what size pieces, not its strength or quality. A No. 1 Common board can be just as sound as an FAS one; it simply has more knots and character. Softwood structural grades are the exception, since those are graded specifically for strength.
Is FAS hardwood worth the extra cost?
Only if you need long, wide, clear sections for tabletops or book-matched panels. For projects with smaller parts or a mix of visible and hidden surfaces, buying some FAS and some No. 1 Common saves money with no visible difference in the finished piece.
Can I use construction-grade lumber for furniture?
Yes, especially for painted or rustic projects. Standard No. 2 pine works fine for face frames, drawer boxes, and structural parts, and the knots add character for farmhouse-style builds. Just avoid loose knots and fill any voids before finishing.
What does S4S mean on lumber pricing?
S4S means surfaced four sides: the lumber has been planed smooth on all four faces. This is standard for softwood dimension lumber but costs extra for hardwoods, which are usually sold rough. S2S means only the two faces are planed, with the edges left rough.
Why is quartersawn lumber more expensive?
Quartersawn cutting yields less usable lumber per log and takes more labor, but it produces more dimensionally stable boards with distinctive grain, like the ray fleck in oak. It is worth the premium for tabletops and drawer fronts that need to stay flat.
How much waste should I expect from No. 1 Common?
Plan for roughly 15 to 25% waste when cutting around defects, though it varies with the board and how you cut it. Waste can be minimal for small parts and higher for long, wide pieces, so buy 20 to 30% extra to be sure of enough usable yield.
Dave Spencer teaches woodworking fundamentals without the fluff. Creator of WoodworkingForAmateurs.com, where beginners learn what actually works instead of what sounds impressive. Believes the best project is the one you finish, not the one you abandon chasing perfection. Former contractor who’s made every mistake in the book so you don’t have to.