The blade that came on your bandsaw is a compromise, chosen by the factory to do a little of everything and none of it especially well. That is fine until you try to slice a thick board into two thinner ones and the cut wanders like a drunk, or you try to follow a tight curve and the blade binds and stalls. Those two jobs, resawing and cutting curves, want almost opposite blades, and no single blade does both well.
Picking the right one comes down to two numbers printed on the box: width and teeth per inch. Get those right for the cut in front of you and the saw suddenly feels like a different, better machine. Here is how each number works, why resawing and curves pull in opposite directions, and what to put on the saw for each.
The Three Numbers on a Bandsaw Blade
A bandsaw blade is sold by three specs, and two of them do most of the deciding.
Width is the distance across the blade, from the tooth tips to the back edge, usually from 1/8 inch up to 3/4 inch or an inch on larger saws. Width controls two things at once: how straight the blade tracks through a cut, and how tight a curve it can turn. Those two work against each other, which is the whole heart of the resaw-versus-curves question.
Teeth per inch, or TPI, is how many teeth fall in each inch of blade. Fewer, larger teeth cut fast and clear big chips; more, smaller teeth cut slower and smoother. The right count depends mostly on how thick the material is.
The third spec is tooth form and rake, including the hook angle of the teeth. It matters, but it gets its own treatment, and if you want to understand why a hook-tooth blade cuts so differently from a regular one, the hook angle is the place to start. For picking a blade by job, width and TPI carry the load.
Width: Straight Tracking vs. Tight Turns
A wide blade is a straight-line tool. The extra width across the blade resists sideways deflection, so it holds its line through a deep cut instead of bowing off course. That is exactly what resawing needs: a tall, straight cut down the length of a board with no wander. The widest blade your saw can properly tension is almost always the right resaw blade.
A narrow blade does the opposite. It cannot track a long straight cut nearly as well, but it can turn. The narrower the blade, the tighter the radius it can follow, because a wide blade binds in a curve the moment the wood tries to turn faster than the blade’s back can clear. Every blade width has a practical minimum radius, and it climbs fast as the blade gets wider.
| Blade width | Tightest radius (approx.) | Typical role |
|---|---|---|
| 1/8″ | 3/16″ | tight scrollwork |
| 3/16″ | 5/16″ | tight curves |
| 1/4″ | 5/8″ | general curves (all-rounder) |
| 3/8″ | 1-1/2″ | gentle curves, light resaw |
| 1/2″ | 2-1/2″ | resaw, very gentle curves |
| 3/4″ | 5-1/2″ | resaw only |
The bars show how quickly the turning radius opens up. Going from a 1/4-inch to a 1/2-inch blade roughly quadruples the tightest curve you can follow, and a 3/4-inch resaw blade cannot cut anything you would call a curve. These are rules of thumb, not exact limits; a sharp blade and a slow feed buy you a little, and forcing a tighter turn than the width allows just twists and binds the blade.
TPI: Matching Teeth to the Thickness
TPI is set by thickness, and two opposite rules decide it. The first: you want at least three teeth in the wood at any moment, or the blade grabs and stutters instead of cutting. Thin stock gives teeth little material to sit in, so it needs a higher tooth count to keep enough teeth engaged. The second: in thick stock, each tooth has to carry its chip a long way before it clears the wood, and the space between teeth, the gullet, has to be big enough to hold that chip. Big gullets mean fewer, larger teeth, so thick cuts want a low tooth count.
Those two rules point in opposite directions, and thickness decides which one wins. For thin material the three-teeth rule dominates and you go higher, roughly 10 to 14 TPI. For thick resawing, gullet clearance dominates and you go low, 2 to 3 TPI, so the gullets can haul the long chips out without packing solid and burning. In between, 4 to 6 TPI covers most everyday cutting in three-quarter-inch stock. Aim for something like three to six teeth in the cut and you will rarely be far off.
Two Jobs, Two Blades
Put the two numbers together and the blades for the two jobs almost design themselves.
For resawing: the widest blade the saw can tension, with a low tooth count of 2 to 3 TPI and a hook tooth for aggressive chip clearance. Half-inch is the common resaw width on mid-size saws; three-quarter-inch or wider on big ones. The wide blade holds the line, the big gullets clear the deep cut, and a blade that is properly tensioned with the drift dialed in tracks straight down a fence. On a smaller saw, a thin-kerf resaw blade earns its price by removing less wood per pass, which strains the motor less and leaves more usable thickness in every slice.
โ Blades Built for Resawing
A wide, low-TPI blade is what turns a frustrating resaw into a clean one. A dedicated resaw blade in the 2 to 3 TPI range clears the deep cut without burning, and a bimetal or thin-kerf version holds an edge longer and wastes less wood on smaller saws.
Resaw Blade (2-3 TPI) Bimetal Resaw BladeFor curves: a blade narrow enough to turn the tightest radius on the part, with a moderate tooth count for the thickness. A 1/4-inch blade handles most furniture curves and still cuts a passably straight line, which is why it is the most common general-purpose blade. Drop to 1/8 or 3/16 inch only when the curve is genuinely tight, since those narrow blades wander badly on anything straight and break more easily.
With the two blades understood, the actual selection is quick:
That last line is where most hobbyists actually land. Changing a bandsaw blade takes a few minutes, and re-tensioning and re-tracking take a few more, so a lot of people leave a 1/4-inch, 4 to 6 TPI blade on the saw and accept that it resaws slowly and cannot cut the tightest curves. That is a reasonable choice. Just know that when a cut fights you, the blade is usually the reason, and swapping to the right one for that job fixes more than fiddling with feed rate and technique ever will.
Common Mistakes
Trying to resaw with the blade that came on the saw. Stock blades are usually around 3/8 inch and 4 to 6 TPI, fine for general work and wrong for resawing. Too narrow to hold the line and carrying too many teeth to clear a deep cut, they wander and burn. Fit a wide, low-TPI blade before you resaw anything tall.
Forcing a wide blade around a tight curve. A 1/2-inch blade will not turn a 1-inch radius, and pushing it just twists the blade, burns the cut, and can pull the blade off the wheels. Match the width to the radius, make relief cuts, or switch to a narrower blade.
Running too many teeth in thick stock. A fine, high-TPI blade in a deep cut packs its gullets solid, and packed gullets stop cutting and start burning. Thick means low TPI. If the cut smokes and slows in thick wood, the tooth count is too high before anything else is wrong.
Over-tensioning a narrow blade to stop it wandering. A 1/8 or 3/16-inch blade cranked past its rating snaps, and it will not track straight no matter the tension, because narrow blades simply are not straight-line tools. A narrow blade wandering on a straight cut is telling you to fit a wider one, not to tension harder.
Ignoring thickness when picking TPI. The same blade that cuts thin plywood cleanly will burn in six-inch resaw stock, and the blade that flies through resaw stock will grab and chatter in thin material. TPI is not a quality setting; it is matched to how thick the wood is.
๐จ Blades for Curves and Everyday Cuts
A narrow blade turns the curves a resaw blade cannot, and a small assortment means you are not stuck cutting shapes with whatever is on the saw. A 1/4-inch blade covers most furniture work; keep a narrower one on hand for tight radii.
Narrow Curve Blade Bandsaw Blade Variety Pack๐ซ Free Woodworking Plans for Beginners
Download step-by-step plans for beginner-friendly builds, including our popular Transformer Bench that converts from a picnic table into a bench and back again.
Download Free Plans โRead Next
Frequently Asked Questions
What width bandsaw blade is best for resawing?
The widest your saw can properly tension, usually 1/2 inch on mid-size saws and 3/4 inch or more on larger ones. A wide blade resists deflection and holds a straight line through the deep cut, which is exactly what resawing needs.
What TPI should I use for resawing?
Low, around 2 to 3 TPI. Resawing is a thick, deep cut, and the large gullets of a low-TPI blade carry the long chips out without packing and burning. A hook tooth form adds the aggressive chip clearance a deep cut wants.
What size blade cuts the tightest curves?
The narrowest one. A 1/8-inch blade turns roughly a 3/16-inch radius, a 1/4-inch blade needs about a 5/8-inch radius, and a 1/2-inch blade wants around 2-1/2 inches. Narrower turns tighter, at the cost of wandering on straight cuts.
Can I use one blade for both resawing and curves?
Not well. The two jobs want opposite blades: wide and coarse for resawing, narrow and finer for curves. If you refuse to swap, a 1/4-inch, 4 to 6 TPI blade is the least-bad compromise, resawing slowly and skipping the tightest curves.
How many teeth should be in the cut?
Roughly three to six at any moment. Fewer than three and the blade grabs and stutters; many more in thick stock and the gullets clog. Because teeth-in-the-cut depends on both TPI and thickness, that range is what actually drives the TPI choice.
Why does my bandsaw blade wander when resawing?
Usually a blade that is too narrow or has too many teeth, not enough tension, or uncorrected drift. Fit the widest low-TPI blade the saw takes, tension it to the blade’s rating, and set the fence to the saw’s natural drift angle before blaming your feed technique.
Dave Spencer teaches woodworking fundamentals without the fluff. Creator of WoodworkingForAmateurs.com, where beginners learn what actually works instead of what sounds impressive. Believes the best project is the one you finish, not the one you abandon chasing perfection. Former contractor who’s made every mistake in the book so you don’t have to.