Buying Rough Lumber vs. S4S: When Extra Milling Is Worth the Savings

Buying Rough Lumber vs. S4S: When Extra Milling Is Worth the Savings
🛠️ Free Woodworking Plans: Build a Transformer Bench that converts from picnic table to bench — Get the free plans →
Estimated Reading Time: 10–12 minutes
woodworker shopping for lumber in home depot” style=

Rough lumber costs 30-50% less per board foot than surfaced lumber, creating appealing savings potential that tempts beginners toward buying rough stock before understanding the implications. The lower price requires owning jointers and planers costing $700-3500 combined, investing time learning milling techniques that have nothing to do with actual project building, and accepting 15-20% material loss to waste during surfacing. For woodworkers with equipment and skills, rough lumber provides both cost savings and control over final dimensions. For beginners or occasional builders, S4S (Surfaced 4 Sides) lumber eliminates equipment needs and gets projects started immediately despite higher per-board-foot costs. The decision isn’t obvious—it depends on project volume, budget, available space, and whether you value time or money more highly.

This guide explains lumber terminology, provides realistic cost comparison accounting for waste, details required equipment and skills, covers thickness expectations, describes the milling workflow, and offers decision frameworks for when each option makes sense.

Understanding the Terminology

Lumber terminology can confuse beginners who encounter various surfacing options without understanding what each means.

Rough Lumber

Rough lumber comes directly from the sawmill with saw marks visible on all surfaces. The boards are approximately the stated thickness—4/4 rough is roughly 1 inch thick, 8/4 is roughly 2 inches—but actual thickness varies and surfaces are uneven. You cannot use rough lumber directly in projects; it requires milling to create flat, smooth, uniform surfaces.

S2S (Surfaced 2 Sides)

S2S lumber has two faces (usually top and bottom) surfaced smooth but edges remain rough. This is less common in hardwoods but appears in some specialty applications. It still requires edge jointing before use.

S4S (Surfaced 4 Sides)

S4S lumber—the most common pre-surfaced option—has all four sides machined smooth and square. It’s ready to cut and use in projects without additional milling. The thickness is consistent and predictable, typically 3/4 inch for 4/4 stock, 1-1/8 inches for 6/4, and 1-3/4 inches for 8/4.

Hit or Miss

Some mills offer “hit or miss” surfacing—boards run through planers but not jointed first. This removes heavy saw marks but doesn’t guarantee flatness. It’s cheaper than true S4S but still needs jointer work before use.

True Cost Comparison

Comparing rough and S4S pricing requires accounting for material waste and equipment costs, not just per-board-foot sticker prices.

Price Per Board Foot

Using red oak as example: Rough 4/4 might cost $5 per board foot. S4S 4/4 runs $7-8 per board foot. The $2-3 difference looks significant—40-60% premium for surfaced lumber.

Waste Factor Reality

Rough 4/4 lumber loses 15-20% of thickness during milling. Starting with nominal 1-inch thickness, you might finish at 13/16 or 7/8 inch after removing saw marks, flattening one face, and creating parallel opposite face. This lost material still costs money—you paid for board feet you can’t use.

For a project requiring 40 board feet of finished lumber, you need to purchase approximately 48 board feet of rough stock to account for waste. At $5/BF rough, that’s $240. The same project using S4S at $7.50/BF costs $300 for exactly 40 usable board feet. The real savings is $60, not the $100 that simplistic math suggests.

Equipment Amortization

A decent benchtop jointer costs $400-800. A benchtop planer costs $300-600. Combined investment: $700-1400 for entry-level equipment, $2000-4000 for quality stationary tools. These costs must amortize across multiple projects before rough lumber becomes truly economical.

If you build one project yearly using 50 board feet, the $60 savings per project means breaking even after 12-23 projects—over a decade of woodworking. For hobbyists building monthly, payback happens within 1-2 years. When calculating these economics, understanding accurate board footage requirements prevents both material shortages and excessive purchasing that wastes money regardless of which lumber type you choose.

Time as Cost

Milling rough lumber adds 30-60 minutes per project—sometimes more for beginners or complex glue-ups. If your time has monetary value (opportunity cost of other activities), factor this into cost comparison. For professionals, milling time is billable hours not spent on client work. For hobbyists with limited shop time, milling eats into actual building time.

💡 Tip: Calculate break-even point for your situation: divide equipment cost by savings per project. If the result exceeds your expected project count over 3-5 years, S4S makes more financial sense despite higher per-unit costs.

Required Equipment and Skills

Successfully milling rough lumber demands both equipment and technique that beginners often underestimate.

The Jointer

Jointers create flat reference faces and square edges. Without a jointer (or hand plane skills to substitute), you cannot effectively mill rough lumber. The jointer is the foundation of the milling process—everything else depends on having one flat face to reference.

6-inch jointers handle boards up to 6 inches wide. 8-inch jointers accommodate wider boards. Bed length affects how well jointers flatten long boards—longer beds (60+ inches) work better than short benchtop models (30-40 inches) for boards over 4 feet.

The Thickness Planer

Planers create uniform thickness and parallel opposite faces. They reference the bottom face—if that face isn’t flat (from jointer work), the planer produces parallel boards that preserve the initial warp. Planers alone cannot flatten warped lumber; they only make both faces parallel to each other.

Benchtop planers (12-13 inch capacity) cost $300-600 and handle most furniture lumber. Larger planers (15-20 inch) cost significantly more but handle wide boards for tabletops and panels.

Hand Plane Alternative

Skilled hand plane users can flatten faces without jointers, substituting hand work for machine work. This requires quality planes, sharpening capability, and developed technique. For woodworkers committed to hand tool work, this eliminates jointer costs but demands time and skill investment.

Most beginners lack hand plane proficiency to flatten boards efficiently. The learning curve is steep, and results vary widely until skills develop. If considering hand plane face jointing, practice extensively on scrap before relying on it for project lumber.

Skill Requirements

Effective jointer use requires understanding grain direction to avoid tearout, recognizing when boards are flat versus still showing twist or bow, and maintaining consistent feed pressure. Planer use is more straightforward but still demands understanding grain direction and proper feed techniques.

Expect 3-5 projects before milling becomes routine rather than challenging. Early projects take longer and produce more waste as you develop technique and judgment.

🛠️ Wood Milling Tools

Essential equipment for processing rough lumber:

Shop Jointers Shop Planers Shop Hand Planes

Thickness Expectations and Planning

Understanding what thickness you’ll actually get from rough lumber prevents project planning mistakes and material shortages.

Standard Rough Thickness

Rough 4/4 (four-quarter, 1 inch nominal) starts around 1-1/16 to 1-1/8 inches actual. Rough 5/4 starts around 1-5/16 inches. Rough 6/4 starts around 1-9/16 inches. Rough 8/4 starts around 2-1/16 inches. These are approximations—individual boards vary.

Expected Finished Thickness

After milling, expect: 4/4 rough → 13/16 to 7/8 inch finished. 5/4 rough → 1-1/16 to 1-1/8 inch finished. 6/4 rough → 1-5/16 to 1-3/8 inch finished. 8/4 rough → 1-13/16 to 1-7/8 inch finished.

The material loss comes from removing saw marks (1/16 inch), flattening one face (1/16-1/8 inch depending on initial warp), and final surfacing to uniform thickness. Heavily warped boards lose more material than straight boards.

Design Implications

If your project requires exactly 3/4-inch thickness, S4S delivers predictably. If you design around rough lumber, plan for 13/16-inch actual thickness from 4/4 stock, or buy 5/4 and mill to 3/4 inch (wasteful but gives you exact thickness).

Alternatively, design projects that accept variable thickness—many furniture designs work with 13/16 or 7/8-inch material instead of requiring precisely 3/4 inch. This flexibility maximizes rough lumber utility.

Thickness Variation Between Boards

Even within single rough lumber purchases, thickness varies. Some 4/4 boards might finish at 7/8 inch, others at 13/16 inch. Plan to mill all boards for a project together, measuring finished thickness, then adjust project designs to accommodate actual dimensions rather than assumed theoretical thickness.

The Milling Workflow

Proper milling sequence produces flat, square, uniformly thick lumber ready for project work.

Step 1: Rough Cutting to Length

Cut rough boards to approximate project lengths plus 2-4 inches excess. This makes handling easier and allows removing defective ends. Don’t final-dimension yet—boards might warp slightly after initial milling.

Step 2: Face Jointing

Run one face across the jointer until it’s completely flat with no twist, cup, or bow. This creates your reference face. Mark this face clearly—all subsequent operations reference it.

For badly warped boards, you might remove significant material creating this flat face. Severe cases might not yield usable thickness—another reason to expect 15-20% waste from rough lumber.

Step 3: Edge Jointing

With the flat face against the jointer fence, joint one edge square to the face. This gives you two reference surfaces (one face, one edge) that are flat and perpendicular. Understanding proper squaring techniques and reference surfaces prevents accumulated errors that create joinery problems later in projects.

Step 4: Planing to Thickness

Run boards through the planer with the jointed face down. The planer creates a face parallel to the bottom reference. Make multiple passes removing 1/16 to 1/8 inch per pass until reaching desired final thickness.

Step 5: Ripping to Width

Use the table saw to rip boards to final width, using the jointed edge against the fence. This creates the fourth square surface, completing the milling process. Now you have S4S lumber ready for cutting to final lengths and joinery work.

Step 6: Final Dimensioning

After milling, let boards rest 24-48 hours if possible. They may move slightly as internal stresses release. Check for any warping, re-joint if necessary, then cut to final project dimensions.

When to Buy Rough Lumber

Specific situations favor rough lumber despite additional work and equipment requirements.

High-Volume Building

If you build multiple projects yearly consuming hundreds of board feet, rough lumber savings compound significantly. The equipment investment amortizes quickly, and milling becomes routine rather than challenging.

Custom Thickness Needs

Projects requiring non-standard thickness (1 inch actual, 1-1/4 inches, 1-1/2 inches) necessitate rough lumber. S4S comes in limited standard thicknesses. Rough stock gives you flexibility to mill whatever dimensions your designs need.

Wide Board Requirements

S4S selection often skews toward narrower boards—mills keep wider boards as rough since S4S inventory requirements favor standard widths. If you need 10-12 inch wide boards regularly, rough lumber provides better selection.

Equipment Already Owned

If you already own jointer and planer for other reasons, the incremental decision favors rough lumber. The equipment investment is sunk cost, so you’re just comparing material prices and time investment.

When to Buy S4S

Many situations favor S4S despite higher per-board-foot costs.

Beginners Without Equipment

Don’t buy rough lumber before you own milling equipment or develop hand plane skills. S4S lets you start building immediately without $1000+ equipment investment and learning curve.

Many beginners assume they’ll eventually buy jointer/planer and justify rough lumber purchases “for when I get the tools.” Then the rough lumber sits unused for months or years while motivation fades. Buy S4S, build projects, develop skills, then reassess equipment needs based on actual experience rather than assumptions. When starting out, focusing on essential core tools gets you building faster than accumulating specialized equipment before you understand your actual work style and needs.

Small Projects Under 20 Board Feet

For small projects, rough lumber savings might be $15-25 total. This doesn’t justify milling time and complexity. S4S gets small projects completed faster with less hassle.

Limited Shop Space

Jointers and planers consume significant floor space (or storage space for benchtop models). If shop space is premium, eliminating these machines by buying S4S frees room for other tools or work area. Understanding smart shop layout for limited spaces might reveal that jointer/planer footprint creates more problems than S4S premium costs.

Time-Constrained Woodworkers

If shop time is limited (few hours weekly), spending 30-60 minutes per project milling lumber is poor time allocation. S4S maximizes time spent on actual project work rather than material preparation.

Projects Requiring 3/4-Inch Exactly

When designs demand precise 3/4-inch thickness and can’t adjust to 13/16 or 7/8 inch, S4S delivers predictably. Milling rough 5/4 down to 3/4 inch wastes significant material just to achieve standard thickness.

💡 Tip: Start with S4S for your first 5-10 projects. This builds woodworking skills without confounding material preparation challenges with joinery and assembly learning curves. Reassess rough lumber after you understand your actual project volume, available time, and commitment level to the hobby.

🛠️ Free Woodworking Plans for Beginners

Download step-by-step plans for beginner-friendly builds, including our popular Transformer Bench that converts from picnic table into a bench and back again.

Download Free Plans →
Affiliate Disclosure: This post may contain affiliate links. If you purchase through these links, we may earn a small commission at no additional cost to you.

FAQ

How much cheaper is rough lumber compared to S4S?

Rough lumber typically costs 30-50% less per board foot than S4S. For example, rough 4/4 oak might be $5/BF while S4S is $7-8/BF. However, rough lumber loses 15-20% to milling waste. The real savings is approximately 20-35% after accounting for material lost to surfacing. For small projects under 20 board feet, savings might not justify milling equipment costs. For large projects or frequent woodworking, savings compound significantly.

Can I mill rough lumber with just a planer, or do I need a jointer too?

You need both jointer and planer, or hand plane skills to substitute for jointer. Planers reference the bottom face—if that face isn’t flat, the planer produces parallel boards that are uniformly warped. The jointer creates the flat reference face and one square edge. Then the planer makes the opposite face parallel. Trying to skip the jointer produces disappointing results. Alternatives include: buying S4S, using hand planes for face jointing, or building a planer sled jig (less effective but possible).

What final thickness should I expect from rough 4/4 lumber?

Rough 4/4 (nominally 1 inch) lumber typically yields 13/16 to 7/8 inch finished thickness after milling. You lose material to: initial surfacing removing saw marks and irregularities (1/16 inch), jointing one face flat (1/16-1/8 inch depending on initial warp), and final planing to uniform thickness. Plan projects assuming 13/16 inch final thickness from 4/4 rough stock. If you need exactly 3/4 inch, buy 5/4 rough or buy S4S already surfaced to 3/4 inch.

Is rough lumber better quality than S4S?

No quality difference exists—both come from same grade pools. Rough and S4S FAS grade contain identical percentage of clear face. The difference is processing: S4S has been jointed and planed at the mill. Some woodworkers prefer rough because they control final dimensions and can orient grain optimally. Others prefer S4S to avoid milling equipment and time investment. Quality depends on grade purchased, not surfacing status.